 Post subject: Old Brown Glue
PostPosted: Mon Nov 15, 2021 5:03 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
I really like this stuff. So easy to use.

Question: is it as good as normal hot hide for bridge attachment??

My planned uses are bridge and fingerboard.

Mike


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Mon Nov 15, 2021 7:47 pm 
Offline
Cocobolo
Cocobolo
User avatar

Joined: Fri Mar 17, 2017 8:42 pm
Posts: 400
First name: Pierre
Last Name: Castonguay
City: Québec, Qc
Country: Canada
Focus: Repair
Status: Professional
Following. I’m not using it as much as I first imagined. I keep it in the fridge and it’s thicker than molasses at this kind of temp. You then have to heat it up to around 120° before it’s usable and then… why not use HHG instead?

I like OBG a whole lot apart from the temp issue, but this might very well be my own fault. I’m waiting for the others to chime in.

Maybe I should keep it at room temp and use it as an everyday glue instead of fish? What’s everyone's experience with OBG?

To the OP… I’d consider OBG just the same as Liquid hide from Titebond as far as bridges… I may be wrong about this but you know, I'm not taking any chances with bridges.


Pierre
Guitares Torvisse

_________________
Pierre Castonguay


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Mon Nov 15, 2021 7:52 pm 
Offline
Koa
Koa

Joined: Wed Feb 17, 2016 8:54 am
Posts: 854
State: Texas
Country: United States
Focus: Repair
Smylight wrote:
To the OP… I’d consider OBG just the same as Liquid hide from Titebond as far as bridges… I may be wrong about this but you know, I'm not taking any chances with bridges.


That is absolutely not the case. I have been using it for bridges for 3 years now. It is far stronger and higher quality than the Titebond garbage.

I've not noticed a difference between it and HHG for bridges. If you don't do a good job of getting the joint fit well it won't stick no matter what type of glue you use.


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Mon Nov 15, 2021 8:15 pm 
Offline
Cocobolo
Cocobolo
User avatar

Joined: Fri Mar 17, 2017 8:42 pm
Posts: 400
First name: Pierre
Last Name: Castonguay
City: Québec, Qc
Country: Canada
Focus: Repair
Status: Professional
DanKirkland wrote:
Smylight wrote:
To the OP… I’d consider OBG just the same as Liquid hide from Titebond as far as bridges… I may be wrong about this but you know, I'm not taking any chances with bridges.


That is absolutely not the case. I have been using it for bridges for 3 years now. It is far stronger and higher quality than the Titebond garbage.

I've not noticed a difference between it and HHG for bridges. If you don't do a good job of getting the joint fit well it won't stick no matter what type of glue you use.

Hey Dan, happy to get a documented opinion about this.

I get from what you're saying that the main difference with HHG would be in longer open working time, without any drawbacks from the added urea? Is that your opinion from experience?

I know the Titebond LH gets quite a bad rap, but before I turned to fish as my go-to "bench glue" I used it quite a bit for low-stress applications and never had a problem with it, but yeah, I moved on fearing problems down the line.

Also, do you keep it at room temp so it’s readily usable on your bench? It's quite thick even at room temp, so you have to heat it up anyway, don't you?

_________________
Pierre Castonguay


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Mon Nov 15, 2021 8:50 pm 
Offline
Koa
Koa

Joined: Wed Feb 17, 2016 8:54 am
Posts: 854
State: Texas
Country: United States
Focus: Repair
Smylight wrote:
Hey Dan, happy to get a documented opinion about this.

I get from what you're saying that the main difference with HHG would be in longer open working time, without any drawbacks from the added urea? Is that your opinion from experience?

I know the Titebond LH gets quite a bad rap, but before I turned to fish as my go-to "bench glue" I used it quite a bit for low-stress applications and never had a problem with it, but yeah, I moved on fearing problems down the line.

Also, do you keep it at room temp so it’s readily usable on your bench? It's quite thick even at room temp, so you have to heat it up anyway, don't you?


Yes the open time with OBG is much higher therefore much easier to work with too. You can heat it up if you want but I just use it at room temp. Brushes are good for spreading it around when it's cold and thicker. The urea seems to lower the gram strength of it a bit but not nearly enough to create a problem. When I was first getting into hide glue I once made my own from rawhide dog chews (the kind you can get in bulk) and while it was very strong it had maybe a 5-8 second open time which was awful to work with trying to clamp things together.

Fish glue I have seen fail quite a few times. It's good for certain things that aren't under stress but if you can use hide glue with OBG or HHG I always recommend it.


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Mon Nov 15, 2021 10:04 pm 
Offline
Cocobolo
Cocobolo
User avatar

Joined: Fri Mar 17, 2017 8:42 pm
Posts: 400
First name: Pierre
Last Name: Castonguay
City: Québec, Qc
Country: Canada
Focus: Repair
Status: Professional
DanKirkland wrote:
Smylight wrote:
Hey Dan, happy to get a documented opinion about this.

I get from what you're saying that the main difference with HHG would be in longer open working time, without any drawbacks from the added urea? Is that your opinion from experience?

I know the Titebond LH gets quite a bad rap, but before I turned to fish as my go-to "bench glue" I used it quite a bit for low-stress applications and never had a problem with it, but yeah, I moved on fearing problems down the line.

Also, do you keep it at room temp so it’s readily usable on your bench? It's quite thick even at room temp, so you have to heat it up anyway, don't you?


Yes the open time with OBG is much higher therefore much easier to work with too. You can heat it up if you want but I just use it at room temp. Brushes are good for spreading it around when it's cold and thicker. The urea seems to lower the gram strength of it a bit but not nearly enough to create a problem. When I was first getting into hide glue I once made my own from rawhide dog chews (the kind you can get in bulk) and while it was very strong it had maybe a 5-8 second open time which was awful to work with trying to clamp things together.

Fish glue I have seen fail quite a few times. It's good for certain things that aren't under stress but if you can use hide glue with OBG or HHG I always recommend it.

Great, thanks.

I have just gotten some OBG that I had poured into a small bottle out of the fridge, dunked it into my hot water bath warmer and presto, 10 minutes later it was workable. Still not nearly liquid enough as my HHG from this morning, but I could have waited a bit more to get temp higher still. This was much faster anyway than getting precooked HHG cubes from the freezer. I used it to finish a job I had started with fish just this afternoon. I found OBG to have quite a bit more tack than fish but it still allowed for parts to be moved around a bit before settling. I liked it. Never had a problem with fish for lower-stress glue-ups but then I never tried it on bridges, headstock cracks and such.

I'm going to have a go with OBG as my bench glue for a few weeks I think. Thanks for your helpful comments, Dan.


Pierre
Guitares Torvisse

_________________
Pierre Castonguay


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Tue Nov 16, 2021 12:14 am 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Fri Jan 22, 2010 9:59 pm
Posts: 3595
First name: Dennis
Last Name: Kincheloe
City: Kansas City
State: MO
Country: USA
Focus: Build
Status: Amateur
I use it for box closing and binding, and don't treat it any differently than regular HHG. Heat it in the glue pot before application, and reheat after getting the clamps on. Particularly with binding, regular HHG gets quite messy with lumps of gel everywhere. OBG squeezes out pretty well even after it cools, but still a little more comes out after reheating, so I wouldn't be comfortable using it at room temperature. Though I didn't reheat the first time I used it for box closing, and it still held ok. But it also made me nervous that the squeeze-out never completely dried (even after weeks), just turned sort of rubbery. It seems to form a waterproof film on the surface when exposed to air, which burns off when reheated and doesn't re-form (then it dries hard like regular HHG). It's actually quite useful, since it slows the drying time while working. Even without worrying about the gel time, HHG is still a bit of a hurry to get to the reheating step before it dries out.


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Tue Nov 16, 2021 12:17 am 
Offline
Cocobolo
Cocobolo
User avatar

Joined: Fri Mar 17, 2017 8:42 pm
Posts: 400
First name: Pierre
Last Name: Castonguay
City: Québec, Qc
Country: Canada
Focus: Repair
Status: Professional
DennisK wrote:
I use it for box closing and binding, and don't treat it any differently than regular HHG. Heat it in the glue pot before application, and reheat after getting the clamps on. Particularly with binding, regular HHG gets quite messy with lumps of gel everywhere. OBG squeezes out pretty well even after it cools, but still a little more comes out after reheating, so I wouldn't be comfortable using it at room temperature. Though I didn't reheat the first time I used it for box closing, and it still held ok. But it also made me nervous that the squeeze-out never completely dried (even after weeks), just turned sort of rubbery. It seems to form a waterproof film on the surface when exposed to air, which burns off when reheated and doesn't re-form (then it dries hard like regular HHG). It's actually quite useful, since it slows the drying time while working. Even without worrying about the gel time, HHG is still a bit of a hurry to get to the reheating step before it dries out.

Hey Dennis,

How do you go about reheating?


Pierre
Guitares Torvisse

_________________
Pierre Castonguay


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Tue Nov 16, 2021 1:24 am 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Fri Jan 22, 2010 9:59 pm
Posts: 3595
First name: Dennis
Last Name: Kincheloe
City: Kansas City
State: MO
Country: USA
Focus: Build
Status: Amateur
Smylight wrote:
Hey Dennis,

How do you go about reheating?

Hold it over an open flame on the kitchen stove. Keep it moving so as not to char any edges :)


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Tue Nov 16, 2021 3:18 am 
Offline
Old Growth Brazilian Rosewood
Old Growth Brazilian Rosewood
User avatar

Joined: Fri Nov 02, 2007 9:49 am
Posts: 13387
Location: Ann Arbor, Michigan
First name: Hesh
Last Name: Breakstone
City: Ann Arbor
State: Michigan
Country: United States
Status: Professional
It' don't mean a pile of poo if it ain't hot hide glue.


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Tue Nov 16, 2021 5:41 am 
Offline
Contributing Member
Contributing Member

Joined: Tue Dec 17, 2013 10:52 pm
Posts: 3072
First name: Don
Last Name: Parker
City: Charleston
State: West Virginia
Zip/Postal Code: 25314
Country: USA
Focus: Build
Status: Amateur
I come at this question from a slightly different angle. Let me explain.

Old Brown Glue (OBG) is great stuff in that we know what is in it. It’s hot hide glue with enough urea added to make it a gooey liquid at room temperature. Not all store-bought glues are that simple.

My perspective is that you should add enough urea to hot hide glue in order to accomplish the task at hand, but not add any more than that. Why limit the amount of urea? Because the glue doesn’t really act exactly like hot hide glue when it has an excessive amount of urea in it. It’s glue, but it doesn’t work like hot hide glue. It takes a long time to firm up (if it ever does), and I can’t say for sure, but it feels less secure. So, I only add that much urea when I need a super long open time, like when I’m constructing a rosette or custom purfling.

For something like a bridge, I don’t need any urea; I can get the joint glued up in seconds. If I don’t need it, I don’t use it. Or if I had a concern about having enough time, I would maybe add enough urea to make up 5% of the weight of the dry glue I used to make the batch. But OBG has a lot more urea than 5%. For me, it is not the right glue for this particular job; it has way more urea than this job could ever need.

Then there is the cost of OBG, as compared to making your own. You really are paying a lot more for having it come in a premixed bottle. And you have to keep your eye on the expiration date, which is not a concern when you make it yourself.

If somebody gave me a fresh bottle of OBG for free, I would gladly use it for those hot hide glue jobs where I need a super long open time. But gluing on a bridge is not in that category, so I wouldn’t use it for that. I’m sure there are folks who successfully glue on bridges with it; I just wouldn’t go that route myself, for the reasons stated.



These users thanked the author doncaparker for the post (total 3): Mike OMelia (Wed Nov 17, 2021 4:50 pm) • Smylight (Tue Nov 16, 2021 8:45 am) • Robbie_McD (Tue Nov 16, 2021 8:34 am)
Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Wed Nov 17, 2021 4:48 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
Well, I like to ask this question every so often to see if there are adherents. Someone here seemed to like it. But most are wary. I think I have my answer. I’ll start using HHG for bridge and finger board extension.

Thank you.

Mike



These users thanked the author Mike OMelia for the post: Smylight (Wed Nov 17, 2021 8:24 pm)
Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Wed Nov 17, 2021 4:50 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
DennisK wrote:
Smylight wrote:
Hey Dennis,

How do you go about reheating?

Hold it over an open flame on the kitchen stove. Keep it moving so as not to char any edges :)


Sounds like a great idea. laughing6-hehe


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Fri Nov 19, 2021 2:04 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Tue May 13, 2008 10:44 am
Posts: 6256
Location: Virginia
It's really quite easy to make your own HHG extend, shall we call it? I use canning salt. I cannot remember the exact weight percent off the top of my head but basically you mix in salt while you cook the hide glue. It doesn't take much and what you end up with is HHG with considerably longer open time. At room temperature the glue is not a liquid but when you heat it up it's a nice running honey liquid and stays open long enough to glue a back on. I use it for just about everything now.


Top
 Profile  
 
 Post subject: Re: Old Brown Glue
PostPosted: Fri Nov 19, 2021 2:44 pm 
Offline
Contributing Member
Contributing Member

Joined: Tue Dec 17, 2013 10:52 pm
Posts: 3072
First name: Don
Last Name: Parker
City: Charleston
State: West Virginia
Zip/Postal Code: 25314
Country: USA
Focus: Build
Status: Amateur
I don't use my preferred "extender" (urea) all the time, but as I mentioned above, if I have any concern about having enough time to get the clamps on, I will add urea that weighs 5% of whatever amount of dry glue I used to make up the batch. That extends the pre-gel time long enough to where clamping time is really not something to worry about, and it is not enough urea to make the glue act weird. It just extends the pre-gel time with no bad side effects. Pretty handy.



These users thanked the author doncaparker for the post: Barry Daniels (Sat Nov 20, 2021 11:29 am)
Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 15 posts ] 

All times are UTC - 5 hours


Who is online

Users browsing this forum: No registered users and 51 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com