Official Luthiers Forum!

Owned and operated by Lance Kragenbrink
It is currently Thu Nov 28, 2024 6:04 am


All times are UTC - 5 hours





Post new topic Reply to topic  [ 5 posts ] 
Author Message
 Post subject:
PostPosted: Tue Jul 10, 2007 2:05 pm 
Offline
Koa
Koa
User avatar

Joined: Wed Apr 18, 2007 6:46 am
Posts: 1012
Location: Issaquah, Washington USA
I have a chance to pick up some koa from a recently cut tree.  How long must it be air-dried before I can use it in an instrument?

_________________
A higher purpose for wood.
Rich Smith
Issaquah, WA


Top
 Profile  
 
 Post subject:
PostPosted: Tue Jul 10, 2007 2:34 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Thu May 12, 2005 5:46 am
Posts: 2969
Location: United States
The general rule is 1 year/inch. So thinner sections help you. make sure that the ends are sealed and I'd check it with a moisture meter. You want about 8% or so at 45% rh.
Everyone then thinks longer is better, I'm not really sure why as it seems to me once the wood has hit equilibrium moisture content (emc) it should be stable. Wood does age however, I believe this is the hardening of the woods resins. But it should be workable once it's at emc.
Maybe someone else can enlighten us on this point.
Grab it, sticker it and stash it!

_________________
Jim Watts
http://jameswattsguitars.com


Top
 Profile  
 
 Post subject:
PostPosted: Tue Jul 10, 2007 3:01 pm 
Offline
Walnut
Walnut

Joined: Tue Feb 20, 2007 1:27 pm
Posts: 34
Location: United States

If you are in Hawaii, the lowest % when seasoned/air dried is about 12-16%. no matter how long you sticker it. And Jim is right at 1 year/inch. The figure/color in Koa becomes more pronounced/rich as time goes by after processing. 


ckp.



Top
 Profile  
 
 Post subject:
PostPosted: Tue Jul 10, 2007 3:14 pm 
Offline
Koa
Koa
User avatar

Joined: Wed Apr 18, 2007 6:46 am
Posts: 1012
Location: Issaquah, Washington USA
If the stuff has already been resawn down to approx 1/8" how long will it take to use it - 1/8 of a year?

_________________
A higher purpose for wood.
Rich Smith
Issaquah, WA


Top
 Profile  
 
 Post subject:
PostPosted: Tue Jul 10, 2007 4:25 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Thu May 12, 2005 5:46 am
Posts: 2969
Location: United States
Approximately, but 12% to 16% is too high unless the instrument is going to stay in Hawaii. The other thing to watch for is drying too fast which can create stress and cause cracks. Saw mills will often water their logs to slow it down and help prevent cracking. Maybe one of our sawyers will come along and enlighten us.
Where's Shane when you need him

_________________
Jim Watts
http://jameswattsguitars.com


Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 5 posts ] 

All times are UTC - 5 hours


Who is online

Users browsing this forum: No registered users and 27 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com