PostPosted: Sat Aug 16, 2008 1:03 am 
Offline
Mahogany
Mahogany

Joined: Thu Nov 03, 2005 2:03 pm
Posts: 85
Location: Australia
I applied 4 heavy coats of nitro 2 weeks ago, and we have had very wet & humid condtions since, so I have not been able to get outside to do the second round of coats.
I haven't been able to find any info on issues with delaying further coats. Is it going to matter if it doesn't happen for 3 weeks?
I did cut back/level the day after the first coats.
Frank


Top
 Profile  
 
PostPosted: Sat Aug 16, 2008 2:53 am 
Offline
Koa
Koa

Joined: Mon Jul 02, 2007 1:22 pm
Posts: 766
-


Last edited by TonyFrancis on Mon Dec 02, 2013 9:58 pm, edited 1 time in total.

Top
 Profile  
 
PostPosted: Sat Aug 16, 2008 9:56 am 
Offline
Cocobolo
Cocobolo

Joined: Tue Nov 27, 2007 2:36 am
Posts: 241
Location: Magnolia, Texas
First name: Chuck
Last Name: Gilbert
Focus: Build
Status: Semi-pro
I am using Behlen's Stringed Instrument Lacquer and the label instructions say to use it at full strength over one coat of sealer and to build up to 5 coats at least one hour apart sanding with 360-400 grit between coats. Does anyone know if there's anything so different about this product that allows this type of application? This is only the second guiitar I've used it on and the first one came out OK, but I'm inexperienced at this and maybe it only looks OK to me. idunno

Chuck


Top
 Profile  
 
PostPosted: Sat Aug 16, 2008 4:27 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Fri Aug 19, 2005 4:02 am
Posts: 3263
Location: The Woodlands, Texas
First name: Barry
Last Name: Daniels
There's not that much difference there. Lacquer is so flexible that you can apply it with a wide variety of schedules and it will still come out just fine. Two coats a day with sanding in between, or five coats a day with no sanding until the next set. There really isn't that much difference. Try a few things and see what works best for you and your equipment.


Top
 Profile  
 
PostPosted: Sat Aug 16, 2008 7:35 pm 
Offline
Mahogany
Mahogany

Joined: Thu Nov 03, 2005 2:03 pm
Posts: 85
Location: Australia
ToddStock wrote:
I think wet coat gets confused with heavy coat - you want a wet coat to allow the lacquer to flow out and minimize sanding, as well as achieve a good burn into the previous coats.


I think you are right - wet would have been a better choice of word.
This is only my 4th guitar, and my second using spray equipment with nitro, so I am still feeling my way. On the previous guitar, I simply wasn't getting enough material on and had constant problems with sanding through, particularly on the edges (binding area), reflecting poor technique and uncertainty about how much was enough. Hence my question in a different post last week asking how much lacquer people use on average on a dreadnought. I just know now that I am getting better application, with no sand throughs after 4 coats, and only a couple of small runs which sanded out fine. So the coats are definitely heavier than last time, but 'wet' would have been a better choice. Thanks for your insight.
Frank


Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 6 posts ] 

All times are UTC - 5 hours


Who is online

Users browsing this forum: Colin North, stumblin and 57 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com