PostPosted: Sun Mar 26, 2023 7:06 am 
Offline
Koa
Koa
User avatar

Joined: Sat Jan 19, 2013 7:33 am
Posts: 1876
First name: Willard
Last Name: Guthrie
City: Cumberland
State: Maryland 21502
Zip/Postal Code: 21502
Country: United State
Focus: Repair
Status: Semi-pro
Corrosion on EVO seems to be pretty variable. Despite a finishing process that saw P400/P600/P800/1200 Imperial wet/dry and machine buff (sewn 8" medium wheel and med/fin compound) to mirror-like shine, we saw everything between the dull brown of old brass frets and more of what Mr. Breakstone showed on the Martin with factory-installed EVO after a few months out in the wild. I suspect this may be the usual sort of combination of intention, habit, and happenstance: atmospheric acidity courtesy of geographic location, perspiration pH and player pre- and post-play routine (hands washed, fretboard wipe-down, etc.), base level of sheen, player left hand use, phase of moon, variation in local acceleration due to gravity and the three body problem, and a few other things which I have forgotten.

Corrosion of EVO wire versus nickel silver and stainless was most certainly a topic of conversation at Greenridge, along with all the other stuff seen on customer guitars that seemed to defy rational explanation. The discussion usually came down to head-scratching and authorization of a medicinal spirit ration.

_________________
For the times they are a changin'

- Bob Dylan



These users thanked the author Woodie G for the post (total 3): joshnothing (Sun Mar 26, 2023 4:23 pm) • Hesh (Sun Mar 26, 2023 8:53 am) • Robbie_McD (Sun Mar 26, 2023 7:52 am)
Top
 Profile  
 
PostPosted: Sun Mar 26, 2023 7:45 am 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Sun Mar 30, 2008 8:20 am
Posts: 5968
The demise of EVO wire is a boon to the guitar repair trade. With a little bit of persuasion a client can be convinced the "ping" of stainless is unbearable and their only choice is nickel silver, with the resultant need for fret dressings and - not so eventual - replacement. The "Major Appliance Trade" has learned this lesson, and rather than producing appliances that will last 30 years as they once did, they have convinced people that replacing refrigerators, ranges, washer/dryers, and heat pumps on a 6 to ten year (or less) cycle is normal.
When are guitar makers and repair shops going to start selling extended warrantees so the buyer can prepay for service they may not need? Lets get with the program people! gaah laughing6-hehe



These users thanked the author Clay S. for the post (total 3): Hesh (Sun Mar 26, 2023 8:56 am) • Chris Pile (Sun Mar 26, 2023 8:35 am) • Robbie_McD (Sun Mar 26, 2023 7:52 am)
Top
 Profile  
 
PostPosted: Sun Mar 26, 2023 8:55 am 
Offline
Old Growth Brazilian Rosewood
Old Growth Brazilian Rosewood
User avatar

Joined: Fri Nov 02, 2007 9:49 am
Posts: 13387
Location: Ann Arbor, Michigan
First name: Hesh
Last Name: Breakstone
City: Ann Arbor
State: Michigan
Country: United States
Status: Professional
Woodie G wrote:
Corrosion on EVO seems to be pretty variable. Despite a finishing process that saw P400/P600/P800/1200 Imperial wet/dry and machine buff (sewn 8" medium wheel and med/fin compound) to mirror-like shine, we saw everything between the dull brown of old brass frets and more of what Mr. Breakstone showed on the Martin with factory-installed EVO after a few months out in the wild. I suspect this may be the usual sort of combination of intention, habit, and happenstance: atmospheric acidity courtesy of geographic location, perspiration pH and player pre- and post-play routine (hands washed, fretboard wipe-down, etc.), base level of sheen, player left hand use, phase of moon, variation in local acceleration due to gravity and the three body problem, and a few other things which I have forgotten.

Corrosion of EVO wire versus nickel silver and stainless was most certainly a topic of conversation at Greenridge, along with all the other stuff seen on customer guitars that seemed to defy rational explanation. The discussion usually came down to head-scratching and authorization of a medicinal spirit ration.


Woodie I appreciate your posts a great deal and wanted to thank you for them! Dave and I never thought of the medicinal spirit ration but that's a very good idea! :) We did have a student who is an OLFer bring us some moonshine and I did finish it off but it took me a year to do so :)



These users thanked the author Hesh for the post: Woodie G (Mon Mar 27, 2023 5:46 am)
Top
 Profile  
 
PostPosted: Sun Mar 26, 2023 10:52 am 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Sun Mar 06, 2011 12:04 am
Posts: 5823
First name: Chris
Last Name: Pile
City: Wichita
State: Kansas
Country: Good old US of A
Focus: Repair
Status: Professional
So... a player I know near Miami claims Rick Turner used ceramic frets a couple times on some guitars. Anyone have a source on that story? I did a quick search and got returns on ceramic flatware and StewMac stainless fretwire.

_________________
"Act your age, not your shoe size" - Prince


Top
 Profile  
 
PostPosted: Sun Mar 26, 2023 3:27 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Apr 16, 2012 12:47 pm
Posts: 2522
First name: Jay
Last Name: De Rocher
City: Bothell
State: Washington
Rick Turner and ceramic frets are mentioned in this old Mandolin Cafe thread: https://www.mandolincafe.com/forum/archive/index.php/t-10809.html
"I think ceramic frets are for He Who Has Everything and still needs more. They are literally a high-tech and high-fired ceramic, preshaped and end-dressed for a specific board. Contact Rick Turner at Renaissance Guitars here in Santa Cruz, he's been doing a few guitars with them, so he actually has developed the tooling for installing them (you can't pound them into a slot with a hammer)."

Also: https://www.banjohangout.org/archive/328193
"When I visited Rick Turner in his shop, he showed me a guitar he had just flawlessly fretted with white ceramic material. ( similar material to ceramic honing rods ) It would without doubt be the longest wearing, but I don't know where he gets it. And it must be very difficult to work with. "

Aha! Paydirt: https://www.fleamarketmusic.com/bulletin/bulletin-nonpop.asp?BulletinID=20280
"Posted By: Rick Turner Date: 9/12/2007 8:13:23 AM
I work with a guy from England who developed the ceramic frets. I've put them in two instruments, and they're great. The issue right now is cost. We really need to get a major manufacturer interested so the quantities can justify the tooling costs.

I'll have one of the prototypes at the NAMM show in January if any of you are coming and want to see."

_________________
Once in a while you get shown the light in the strangest of places if you look at it right - Robert Hunter



These users thanked the author J De Rocher for the post: Chris Pile (Sun Mar 26, 2023 4:14 pm)
Top
 Profile  
 
PostPosted: Sun Mar 26, 2023 4:15 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Sun Mar 06, 2011 12:04 am
Posts: 5823
First name: Chris
Last Name: Pile
City: Wichita
State: Kansas
Country: Good old US of A
Focus: Repair
Status: Professional
Excellent! Food for thought.

The big problem I see with ceramic frets is dressing the fret ends after installation. Diamond files?

_________________
"Act your age, not your shoe size" - Prince


Top
 Profile  
 
PostPosted: Sun Mar 26, 2023 4:34 pm 
Offline
Koa
Koa

Joined: Tue Jan 15, 2013 10:00 pm
Posts: 985
First name: Josh
Focus: Build
Status: Amateur
Woodie G wrote:
Corrosion on EVO seems to be pretty variable. Despite a finishing process that saw P400/P600/P800/1200 Imperial wet/dry and machine buff (sewn 8" medium wheel and med/fin compound) to mirror-like shine, we saw everything between the dull brown of old brass frets and more of what Mr. Breakstone showed on the Martin with factory-installed EVO after a few months out in the wild. I suspect this may be the usual sort of combination of intention, habit, and happenstance: atmospheric acidity courtesy of geographic location, perspiration pH and player pre- and post-play routine (hands washed, fretboard wipe-down, etc.), base level of sheen, player left hand use, phase of moon, variation in local acceleration due to gravity and the three body problem, and a few other things which I have forgotten.


I had a customer last year who asked me to help him with some spontaneous corrosion issues on a custom telecaster he’d just commissioned from an EU maker. No matter how rigorously he cleaned the instrument after play, upon opening the case for his next session he’d find corroded frets and humbucker covers. Other metal parts of the instrument were unaffected. Some experimentation revealed the problem - off-gassing from the oil varnish finish in the tight confines of the case was causing the tarnishing of nickel components (hb covers, frets) but it had no effect on chrome components (bridge, tuners, control plate). A stainless refret and swap to chrome covers was the solution.



These users thanked the author joshnothing for the post (total 4): Pmaj7 (Mon Mar 27, 2023 10:38 am) • Woodie G (Mon Mar 27, 2023 5:45 am) • Hesh (Sun Mar 26, 2023 7:19 pm) • Robbie_McD (Sun Mar 26, 2023 7:05 pm)
Top
 Profile  
 
PostPosted: Sun Mar 26, 2023 5:24 pm 
Offline
Koa
Koa
User avatar

Joined: Thu Jan 10, 2008 5:08 am
Posts: 1906
Location: Raleigh, NC
First name: Steve
Last Name: Sollod
Focus: Build
Status: Amateur
jfmckenna referenced Cryowire. It sounds like the hardness is between standard wire and stainless. I saw something on youtube that said it was 4 times harder than standard wire. It's supposed to be easy to work. Perhaps it has the qualities that Evo has... (without the gold color and corrosion issues). Are there any thoughts about Cryowire?

_________________
Steve Sollod (pronounced sorta like "Solid")
www.swiftcreekguitars.com



These users thanked the author sdsollod for the post: Pmaj7 (Mon Mar 27, 2023 10:38 am)
Top
 Profile  
 
PostPosted: Mon Mar 27, 2023 6:06 am 
Offline
Koa
Koa
User avatar

Joined: Sat Jan 19, 2013 7:33 am
Posts: 1876
First name: Willard
Last Name: Guthrie
City: Cumberland
State: Maryland 21502
Zip/Postal Code: 21502
Country: United State
Focus: Repair
Status: Semi-pro
On corrosion in the case, not unusual to see Gretsch guitars of a certain age come in with extensive hardware corrosion due to out-gassing of nitric acid from the cellulose nitrate binding. Once that starts, the only remedy is removal of the destabilized cellulose nitrate materials and rebinding, plus possible replacement of the hardware if the plating damage is beyond just the cosmetic.

With EVO, there would need to be a similar acidic vapor or metallic salts + moisture issue, as the material - originally developed to provide a gold-toned eyeglass frame material for those with nickel allergies - is supposed to be fairly corrosion-resistant in constant skin contact situations.

On cryo-treated fret wire... I hesitate to imagine the sheer joy involved in leveling, crowning, and polishing stuff that is harder and tougher than stainless wire. One or two jumbo SS high/wide 118 x 57 refrets per month is my current personal joy limit... any more than that threatens to push me into uncharted territory with regard to my relationship with the sublime. Normal humans are not properly equipped to deal with that much positive emotional energy ;) .

_________________
For the times they are a changin'

- Bob Dylan



These users thanked the author Woodie G for the post (total 4): Smylight (Tue Mar 28, 2023 8:56 am) • joshnothing (Tue Mar 28, 2023 7:20 am) • Hesh (Mon Mar 27, 2023 11:08 am) • Pmaj7 (Mon Mar 27, 2023 10:54 am)
Top
 Profile  
 
PostPosted: Mon Mar 27, 2023 9:31 am 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Tue May 13, 2008 10:44 am
Posts: 6256
Location: Virginia
Hey Hesh did you guys use that sewing machine tester to test Cryowire?



These users thanked the author jfmckenna for the post: Hesh (Mon Mar 27, 2023 11:05 am)
Top
 Profile  
 
PostPosted: Mon Mar 27, 2023 10:54 am 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Sat Jan 15, 2005 12:50 pm
Posts: 3929
Location: United States
Both cellulose nitrate and cellulose acetate release acids as they break down, and are considered by museum conservators as 'toxic' to collections. They have to be isolated to avoid future damage to other objects.



These users thanked the author Alan Carruth for the post: Pmaj7 (Mon Mar 27, 2023 12:28 pm)
Top
 Profile  
 
PostPosted: Mon Mar 27, 2023 10:57 am 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Wed Feb 20, 2008 7:15 pm
Posts: 7380
First name: Ed
Last Name: Bond
City: Vancouver
Country: Canada
Focus: Build
Status: Professional
Are people still using that kind of stuff, or are modern materials better?


Top
 Profile  
 
PostPosted: Mon Mar 27, 2023 11:08 am 
Offline
Old Growth Brazilian Rosewood
Old Growth Brazilian Rosewood
User avatar

Joined: Fri Nov 02, 2007 9:49 am
Posts: 13387
Location: Ann Arbor, Michigan
First name: Hesh
Last Name: Breakstone
City: Ann Arbor
State: Michigan
Country: United States
Status: Professional
jfmckenna wrote:
Hey Hesh did you guys use that sewing machine tester to test Cryowire?


No it sounds like a fad to me that won't last. I also don't understand what problem cryo wire is trying to solve when the stainless frets on some of mine will never wear out for players like me. I mean stainless when it comes to wear can wear out but it's not common and a refret never killed anyone.... ;)


Top
 Profile  
 
PostPosted: Mon Mar 27, 2023 11:27 am 
Offline
Koa
Koa

Joined: Mon Feb 13, 2012 8:49 pm
Posts: 1041
First name: peter
Last Name: havriluk
City: granby
State: ct
Zip/Postal Code: 06035
Country: usa
Focus: Build
Status: Amateur
Wallet fattening.

_________________
Peter Havriluk



These users thanked the author phavriluk for the post: Hesh (Tue Mar 28, 2023 2:50 am)
Top
 Profile  
 
PostPosted: Mon Mar 27, 2023 12:35 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Sat Jan 31, 2009 8:50 pm
Posts: 2257
Location: Seattle WA
Focus: Build
Status: Semi-pro
Hesh wrote:
I also don't understand what problem cryo wire is trying to solve


They are advertising it as being tougher without any extra work. I was assuming they were comparing that to regular fret wire and not stainless.

Pat

_________________
Pat



These users thanked the author Pmaj7 for the post: Hesh (Tue Mar 28, 2023 2:51 am)
Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 40 posts ]  Go to page Previous  1, 2

All times are UTC - 5 hours


Who is online

Users browsing this forum: Bing [Bot], Ken Lewis, Mike Franks and 45 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com