PostPosted: Mon May 29, 2023 9:30 am 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
This article compares various glues (OBG, HHG, PVA, etc). https://www.finewoodworking.com/2007/07 ... -your-glue

The experiment set up seems reasonable. I leave you to decide that. The surprize result was that OBG was as good as HHG. And PVA was very good.

Holding strength is not the only concern in this business. Repairability is a concern too. But I was impressed OBG rated as well as HHG

Mike



These users thanked the author Mike OMelia for the post: Cal Maier (Mon May 29, 2023 9:36 am)
Top
 Profile  
 
PostPosted: Mon May 29, 2023 11:41 am 
Offline
Old Growth Brazilian Rosewood
Old Growth Brazilian Rosewood
User avatar

Joined: Fri Nov 02, 2007 9:49 am
Posts: 13387
Location: Ann Arbor, Michigan
First name: Hesh
Last Name: Breakstone
City: Ann Arbor
State: Michigan
Country: United States
Status: Professional
ballbanjos wrote:
I saw a YouTube video touring the Gib**n custom shop, where OBG (the bottle was being heated in a water filled glue pot) was being used to glue Les Paul tops onto the mahogany backs. Oddly enough, they were using regular HHG from a pot to glue on necks and fingerboards...I guess that must be the only correct way to do it idunno

Dave


So the Gib**n :) custom shop is cheating, no surprise there they were caught red handed poaching...

They advertise that they use HHG on the assembly of the Custom shop Lesters. OBG is not HHG nor is it what they used to assemble Les Pauls in the coveted era of 58 - 60. If I were someone who paid $5K and up into the $11K range for a Murphy Labs, Custom Shop Les Paul and found out that they did not use HHG on my top I would be pissed.

There is a long standing expression that many of us in the business use, "good enough for a Gibson." Makes perfect sense now, again.

Also, before I go this application the drop top is pretty uneventful with tons of wood-to-wood gluing surface and no tension or stresses unless Townshend gets ahold of it. Or, in other words not an application that I would expect any glue to fail in.

To be clear my disgust with Gib**n is with management not the products produced in Kalamazoo. I own two Les Pauls, a Firebird, a 76 ES 175, a 2004 335 and a SG with Lollar high-wind imperials so I b*tch a lot about g*bson but I love em too when no one is looking... :)

Oh and one more comment: As the woodworkers here consider using OBG be aware that no one ever asks a Luthier if you used OBG.... they only seem to look for and ask about HHG.

Tradition in Lutherie is like the force in Star Wars, very, very strong.


Top
 Profile  
 
PostPosted: Mon May 29, 2023 12:20 pm 
Offline
Koa
Koa

Joined: Mon Dec 18, 2006 9:42 am
Posts: 1577
Location: United States
I am pretty ignorant here, but I did read other things on this site about OBG and HHG, I think.

Somewhere, there are posts mentioning how to extend open time for HHG by adding chemicals (urea?). But the posts did not claim that this makes the glue no longer HHG.

Also, for OBG I read that once it dries, it is identical to HHG.

So is OBG just a brand name for a particular formulation of extended HHG?

Just asking.


Top
 Profile  
 
PostPosted: Mon May 29, 2023 12:41 pm 
Offline
Contributing Member
Contributing Member

Joined: Tue Dec 17, 2013 10:52 pm
Posts: 3072
First name: Don
Last Name: Parker
City: Charleston
State: West Virginia
Zip/Postal Code: 25314
Country: USA
Focus: Build
Status: Amateur
https://www.oldbrownglue.com/


Top
 Profile  
 
PostPosted: Mon May 29, 2023 1:21 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
OBG is hide glue mixed with urea (the stuff in pee). Lowers the crystallization temperature. When it dries, it’s still hide glue, but it has urea still in it. (Or salt). It apparently has no impact on strength. But it ain’t the original, so folks will continue to debate. I would LOVE to see a side by side comparison with HHG and OBG for applying bridges. Until I do, it’s HHG or PVA


Top
 Profile  
 
PostPosted: Mon May 29, 2023 2:18 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Fri Aug 19, 2005 4:02 am
Posts: 3263
Location: The Woodlands, Texas
First name: Barry
Last Name: Daniels
The addition of urea does weaken the hhg in relation to the amount added.


Top
 Profile  
 
PostPosted: Mon May 29, 2023 2:38 pm 
Offline
Contributing Member
Contributing Member

Joined: Sun Jul 24, 2005 7:12 am
Posts: 712
Location: United States
doncaparker wrote:
https://www.oldbrownglue.com/

Even if you never intend to use OBG, the videos on the website have a lot of information. Some on HHG and some on OBG. But, geared to furniture repair and veneer, etc.


Top
 Profile  
 
PostPosted: Mon May 29, 2023 2:47 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Wed Feb 20, 2008 7:15 pm
Posts: 7380
First name: Ed
Last Name: Bond
City: Vancouver
Country: Canada
Focus: Build
Status: Professional
I’d be curious to try some of the OBG. If the joint still fails at the wood and not the glue line, would that not make it strong enough by default? I mean, once the glue is stronger than the wood, does more strong count for anything?


Top
 Profile  
 
PostPosted: Mon May 29, 2023 3:42 pm 
Offline
Koa
Koa

Joined: Mon Oct 17, 2011 4:10 pm
Posts: 721
First name: Bob
Last Name: Gramann
City: Fredericksburg
State: VA
Zip/Postal Code: 22408
Country: USA
Focus: Build
Status: Professional
Besides strength, we want our glues to have longevity. Does the presence of the urea make the OBG more likely to absorb water from the atmosphere and eventually fail? Any chemists here that can comment? We know HHG will last a couple of millenniums. PVAs have been around for less than a century, but so far, so good. I had a CA joint last for 40 years strong and then fail—it just dropped apart with no strain on it.

So far, I’ve had good luck with the most recent version of the LMI instrument glue (a PVA, I think). It sets a bit faster than Titebond and cures a bit harder. When it gets thick, it’s time to demote it to fixtures and open a new bottle.


Top
 Profile  
 
PostPosted: Mon May 29, 2023 5:26 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Wed Feb 20, 2008 7:15 pm
Posts: 7380
First name: Ed
Last Name: Bond
City: Vancouver
Country: Canada
Focus: Build
Status: Professional
Good question about longevity, and interesting about the CA…


Top
 Profile  
 
PostPosted: Mon May 29, 2023 6:14 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Tue May 13, 2008 10:44 am
Posts: 6256
Location: Virginia
I'm pretty sure the addition of urea goes way way back in time.

As for Titebond, it's absolutely perfectly suited for guitar building from beginner to master builder, many of whom still use Titebond, some of whom laugh at all of us who use HHG.

There is plain and simply no right or wrong glue to use and some of the best guitars in the world have been built with HHG or Titebond. I would wager a bet that most of us here use TB, HHG, CA, possibly even epoxy on every build we do.



These users thanked the author jfmckenna for the post: Barry Daniels (Tue May 30, 2023 8:25 am)
Top
 Profile  
 
PostPosted: Mon May 29, 2023 9:34 pm 
Offline
Koa
Koa

Joined: Tue Jan 15, 2013 10:00 pm
Posts: 985
First name: Josh
Focus: Build
Status: Amateur
Using TB and laughing at HHG users is a funny concept, I find HHG is faster and easier for most of the areas where it is commonly used on new builds - bracing, joining plates, etc. For these operations, using TB is doing it the hard way. And you get to charge more using HHG :D

There are other operations in guitar making or repair where HHG is certainly more work or more fuss. In many cases HHG has advantages which make it worth using anyhow (bridges is a prominent example) but we all have to work in the way we most enjoy or which is most efficient for us.


Top
 Profile  
 
PostPosted: Mon May 29, 2023 10:35 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Sun Mar 30, 2008 8:20 am
Posts: 5968
ballbanjos wrote:
I saw a YouTube video touring the Gib**n custom shop, where OBG (the bottle was being heated in a water filled glue pot) was being used to glue Les Paul tops onto the mahogany backs. Oddly enough, they were using regular HHG from a pot to glue on necks and fingerboards...I guess that must be the only correct way to do it idunno

Dave


Since the bottle was being heated in a water filled glue pot it's possible the contents were regular HHG and the bottle was just being used for application. I have bought Titebond by the gallon (it's much cheaper that way) and refilled smaller bottles for ease of application. With HHG I use small two ounce applicator bottles heated in a water filled hot pot. It makes the process more convenient.


Top
 Profile  
 
PostPosted: Tue May 30, 2023 3:10 am 
Offline
Koa
Koa
User avatar

Joined: Sat Jan 19, 2013 7:33 am
Posts: 1876
First name: Willard
Last Name: Guthrie
City: Cumberland
State: Maryland 21502
Zip/Postal Code: 21502
Country: United State
Focus: Repair
Status: Semi-pro
I concur... Titebond is a perfectly adequate glue for guitars which will never need repair. For those guitars which will need repair, an adhesive that does not creep both hot and cold and is not a joint contaminant when the time comes to reglue that bridge or top bracing after a heat event (or joints made with thick, creepy glue lines) is preferred. Lots of time to figure out what that glue might be after the first couple of instruments.

Again, adequate is just fine for now, despite lots of glue-related 'whataboutisms' which might be raised. As a bonus, that first guitar will likely become a repair tutorial, so may continue to serve an important roll in the 'you don't know what you don't know until you know it' process of craft education, as well as insight as to the preferences of repair professionals.

_________________
For the times they are a changin'

- Bob Dylan


Top
 Profile  
 
PostPosted: Tue May 30, 2023 5:25 am 
Offline
Koa
Koa
User avatar

Joined: Fri Jun 22, 2007 11:14 am
Posts: 1028
Location: Newland, North Carolina
First name: Dave
Last Name: Ball
Clay S. wrote:
ballbanjos wrote:
I saw a YouTube video touring the Gib**n custom shop, where OBG (the bottle was being heated in a water filled glue pot) was being used to glue Les Paul tops onto the mahogany backs. Oddly enough, they were using regular HHG from a pot to glue on necks and fingerboards...I guess that must be the only correct way to do it idunno

Dave


Since the bottle was being heated in a water filled glue pot it's possible the contents were regular HHG and the bottle was just being used for application. I have bought Titebond by the gallon (it's much cheaper that way) and refilled smaller bottles for ease of application. With HHG I use small two ounce applicator bottles heated in a water filled hot pot. It makes the process more convenient.


True. But since other operations were being done with a regular glue pot, and the fact that they happened to have an OBG bottle hanging around makes me doubt that.

Dave



These users thanked the author ballbanjos for the post: Hesh (Tue May 30, 2023 8:07 am)
Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 40 posts ]  Go to page Previous  1, 2

All times are UTC - 5 hours


Who is online

Users browsing this forum: No registered users and 51 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com